Place of Origin: China

Brand Name: Tankii

Model Number: 1cr20al3 0cr25al5 0Cr21Al6Nb

Payment & Shipping Terms

Minimum Order Quantity: 10kg

Price: 5usd/kg

Packaging Details: Standard

Delivery Time: 5-15days

Payment Terms: L/C, D/P, T/T, Western Union

Supply Ability: 100ton/month

Get Best Price
Contact Now
Specifications
Highlight:

0Cr21Al6Nb Round Bar

,

Hot Rolled Mold Steel Round Bar

Description
1cr20al3 0cr25al5 0Cr21Al6Nb Superalloy Round Bar Hot Rolled Mold Steel

Product Description

Best Price 1cr20al3 0cr25al5 0Cr21Al6Nb Superalloy Round Bar Hot Rolled Mold Steel

1Cr13Al4, 0Cr25Al5, 0Cr23Al5, 0Cr21Al6, 0Cr21Al4, 0Cr21Al6Nb, 0Cr27Al7Mo2 is one kind of normal material of Fe-Cr-Al alloy.
FeCrAl alloy has the characteristic of high resistivity,low temperature resistance coefficient,high operating temperature,goodanti-oxidation and anti-corrosion under high temperature.
It is widely used in industrial furnace, household appliances, industry furnace, metallurgy, machinery, aircraft, automotive,
For other industries producing heating elements and resistance elements.
0Cr21Al6Nb
Chemical Content(%)
C P S Mn Si Cr Ni Al Fe Other
Max
0.05 0.025 0.025 0.70 Max 0.6 21.0~23.0 Max 0.60 5.0~7.0 Bal. Nb 0.5
Mechanical Properties
Max Continuous Service Temp 1350ºC
Resisivity at 20ºC 1.45 ohm mm2/m
Density 7.1 g/cm3
Thermal Conductivity 46.1 KJ/m·h·ºC
Coefficient of Thermal Expansion 16.0×10-6/ºC
Melting Point 1510ºC
Tensile Strength 637~784 Mpa
Elongation Min 12%
Section Variation Shrink Rate 65~75%
Repeatedly Bend Frequency Min 5 times
Continuous Service Time -
Hardness 200-260HB
Micrographic Structure Ferrite
Magnetic Property Magnetic

 
 
Grade
Highest temperature
Resistivity
Melting point
Tensile strength
Elongation
0Cr21Al4
1100ºC
1.23±0.06μΩ.m
1500ºC
750
≥12
0Cr25Al5
1250ºC
1.42±0.07μΩ.m
1500ºC
750
≥12
0Cr21Al6NbCo
1350ºC
1.43±0.07μΩ.m
1510ºC
750
≥12
0Cr27Al7Mo2
1400ºC
1.53±0.07μΩ.m
1520ºC
750
≥10
KSC
1350ºC
1.44±0.05μΩ.m
1510ºC
750
≥16
Cr20Ni80
1200ºC
1.09±0.05μΩ.m
1400ºC
750
≥20
Cr15Ni60
1150ºC
1.12±0.05μΩ.m
1390ºC
750
≥20
Cr20Ni35
1100ºC
1.04±0.05μΩ.m
1390ºC
750
≥20
Cr20Ni30
1100ºC
1.04±0.05μΩ.m
1390ºC
750
≥20
Grade
Chemical composition%
C
P
S
Mn
Si
Cr
Ni
Al
Fe
≤
0Cr21Al4
0.12
0.025
0.025
0.7
≤1.0
17-21
≤0.6
3-4
balance
0Cr25Al5
0.06
0.025
0.02
0.5
≤0.6
23-26
≤0.6
4.5-6.5
balance
0Cr21Al6Nb
0.05
0.025
0.02
0.5
≤0.6
21-23
≤0.6
5-7
balance
0Cr27Al7Mo2
0.05
0.025
0.02
0.2
≤0.4
26.5-27.8
≤0.6
6-7
balance
Cr20Ni80
0.08
0.02
0.015
0.6
0.75-1.6
20-23
balance
<0.5
≤1.0
Cr15Ni60
0.08
0.02
0.015
0.6
0.75-1.6
15-18
55-61
<0.5
balance
Cr20Ni35
0.08
0.02
0.015
1.0
1-3
18-21
34-37
-
balance
Cr20Ni30
0.08
0.02
0.015
1.0
1-3
18-21
30-34
-
balance
 
Shanghai Tankii ALloy Material Co.,Ltd. focus on the production of nichrome alloy, thermocouple wire,fecral alloy,precision alloy,copper nickel alloy,thermal spray alloy etc. in the form of wire,sheet,tape,strip,rod and plate.
We've already got ISO 9001 quality system certificate and approval of ISO 14001 environmental protection system.We own a complete set of advanced production flow of refining,cold reduction,drawing and heat treating etc. We also proudly have independent R&D capacity.
 

Style of supply

 

Best Price 1cr20al3 0cr25al5 0Cr21Al6Nb Superalloy Round Bar Hot Rolled Mold Steel

 
Send your inquiry
Please send us your request and we will reply to you as soon as possible.
Send