Product Details
Place of Origin: Shanghai, China
Brand Name: TANKII
Certification: ISO9001 SGS
Model Number: CuMn7Sn
Payment & Shipping Terms
Minimum Order Quantity: 100 KG
Price: negotiable
Packaging Details: Wooned Case
Delivery Time: 7-20 days
Payment Terms: L/C, T/T, Western Union
Supply Ability: 100 Tons per month
Material: |
Copper Manganese Tin |
Resistivity: |
29 |
Surface: |
Bright Surface |
Manganin: |
CuMn7Sn |
Thickenss: |
0.02- 2.5mm |
Width: |
1.0-600mm |
Application: |
Shunt |
Material: |
Copper Manganese Tin |
Resistivity: |
29 |
Surface: |
Bright Surface |
Manganin: |
CuMn7Sn |
Thickenss: |
0.02- 2.5mm |
Width: |
1.0-600mm |
Application: |
Shunt |
Copper-Manganese-Tin Alloy Strip CuMn7Sn Resistivity 0.29 Resistance shunt Strip with Good
Manganin strips are a common form of the manganin alloy used in various electrical and electronic applications. Manganin strips have the following key characteristics:
Material Composition:
Physical Properties:
Electrical Properties:
Applications:
The combination of stable electrical properties and corrosion resistance makes manganin strips a preferred choice for applications where consistent and reliable resistance values are critical, such as in scientific instrumentation, industrial controls, and metrology.
CHEMICAL COMPOSITION
Mn% | Sn% | Cu% | |
Nominal Composition | 7 | 2.5 | Bal. |
PHYSICAL PROPERTIES
Density g/cm3 | 8.5 |
TCR 10-6/K | ±10 |
Elastic Modulus GPa | 125 |
Thermal Conductivity W/(m·K) | 35 |
Thermal expansion coefficient 10-6/ K | 21.6 |
EMF μV/K | -1 |
MECHANICAL PROPERTIES
State | Yield strength | Tensile strength | Elongation | Hardness |
Mpa | MPa | % | HV | |
R350 | - | 350 | 30 | 70 |
Mechanical Properties Manganin 43
Max Continuous Service Temp | 0-100ºC |
Resisivity at 20ºC | 0.44±0.04ohm mm2/m |
Density | 8.4 g/cm3 |
Thermal Conductivity | 40 KJ/m·h·ºC |
Temp Coefficient of Resistance at 20 ºC | 0~40α×10-6/ºC |
Melting Point | 1450ºC |
Tensile Strength(Hard) | 585 Mpa(min) |
Tensile Strength,N/mm2 Annealed,Soft | 390-535 |
Elongation | 6~15% |
EMF vs Cu, μV/ºC (0~100ºC) | 2(max) |
Micrographic Structure | austenite |
Magnetic Property | non |
Hardness | 200-260HB |
Micrographic Structure | Ferrite |
Magnetic Property | Magnetic |