Product Details
Place of Origin: China
Brand Name: GH3600
Certification: COO, CCPIT
Payment & Shipping Terms
Minimum Order Quantity: 50 kgs
Price: negotiation
Packaging Details: Wooden box
Delivery Time: 25-30 days
Payment Terms: Ex works/ FOB/ CPT
Supply Ability: 30,000 kgs/ month
Condition: |
Bright/ Oxidized Soft/ Hard |
Surface: |
Bright |
Diameter: |
3-50mm |
Shape: |
Strip, Foil, Sheet, Wire, Bar. |
Name: |
Inconel 600 UNS N06600 GH3600 |
Condition: |
Bright/ Oxidized Soft/ Hard |
Surface: |
Bright |
Diameter: |
3-50mm |
Shape: |
Strip, Foil, Sheet, Wire, Bar. |
Name: |
Inconel 600 UNS N06600 GH3600 |
High Temp Alloy Superalloy- GH3600 ( Inconel 600 ) for Thermowell , Catalytic Regenerator
Quick Detail:
|
Name |
Inconel 600 UNS N06600 GH3600
|
Application |
thermowell work in Erosion atmosphere; Anti-chlorine, hydrogen chloride, oxidation and carbonization corrosion; Nuclear reactor |
|
Condition |
Bright/ Oxidized Soft/ Hard |
Feature |
GH3600 for a variety of corrosive media have corrosion resistance. Petrochemical production of catalytic regenerator over 700 ℃ applications alloy 600 is recommended for longer life. |
|
Shape |
Strip, Foil, Sheet, Wire, Bar. |
Standard |
|
Description:
Physical properties
>Density (g/cm3): 8.4
>Melting point (℃): 1370~1425
Chemical composition(%)
|
Grade |
C |
Si |
Mn |
P |
S |
Ni |
Cr |
Cu |
Fe |
|
GH3600 |
≤0.15 |
≤0.5 |
≤ 1 |
≤0.015 |
≤0.015 |
72 |
14~17 |
≤0.5 |
6~7 |
Mechanical properties
|
|
|
Yield Strength (Mpa) |
Tensile Strength (Mpa) |
Elongation, % |
Hardness, HB |
|
GH3600 |
Cold-rolling |
240 |
550 |
30 |
≤195 |
|
As annealed |
180 |
500 |
35 |
≤185 |
Specifications
|
Grade |
GH3600 |
|
Size |
Ф 3~50mm |
|
MOQ |
50 kgs |
|
Condition |
Soft/ Hard; Bright/ Oxidized |
![]()